Investigation of corrosion resistance of Ti-6Al-4V alloy welding zone Welded by TIG method

Document Type : Research Paper

Authors

1 . MSc graduated of Materials Engineering, Department of Petroleum, Mining and Materials Engineering, Islamic Azad University, Central Tehran branch, Tehran, Iran.

2 Assistant prof. of Materials Engineering, Department of petroleum, mining and materials engineering, Islamic Azad University, Central Tehran branch, Tehran, Iran.

Abstract

In this research, the effect of current intensity on the corrosion resistance of Ti-6Al-4V alloy welded by Tungsten-inert Gas (TIG) method was investigated. For this purpose, 3 × 50 × 40 mm specimens were prepared and after preparing the surfaces, in a way but joint two-way single pass in vacuum chamber with inert argon with a flow rate of 70, 80 and 90 A were welded. Microstructural studies of base metal (BM), fusion zone (FZ) and heat affected zone (HAZ) were performed using optical microscopy and scanning electron microscopy (SEM). Then, in order to investigate the corrosion resistance of Ti-6Al-4V welded cross sections, the roots of the welded specimens were examined by potentiostatic polarization in seawater and 3.5% NaCl. The results showed that by increasing the welding current intensity from 70 to 80A, the grain size in the weld area as well as the corrosion rate of the weld area in Ti-6Al-4V alloy increased. By varying the flow intensity from 80 to 90A, the corrosion rate and grain size of the weld zone did not change significantly. The corrosion rate of Ti-6Al-4V alloy in 3.5% NaCl solution compared to seawater revealed that the corrosion rate of alloy in 3.5% NaCl solution is higher than its corrosion rate in seawater.

Keywords


1.       Matthew, J. D., Titanium and Its alloys source book, ASM, 1982.

2.       Lin, J.J., Lv, Y.H., Liu, Y.X., Xu, B.S.,   Sun, Z., Li, Z.G.  and Wu, Y.X. 2016. Microstructural evolution and mechanical properties of Ti-6Al-4V wall deposited by pulsed plasma arc additive manufacturing, Materials and Design, 102: 30–40.

3.       Kashaev, N., Ventzke, V., Fomichev, Fomin, V. F. and Riekehr, S. 2016. Effect of Nd:YAG laser beam welding on weld morphology and  mechanical properties of Ti–6Al–4V butt joints and T-joints , Optic Lasers Engineering, 86: 172–180.

4.       Yu, H.,  Li, F., Yang, J., Shao, J., Wang,  Z. and  Zeng, X. 2018. Investigation on laser welding of selective laser melted Ti-6Al-4V parts: Weldability, microstructure and mechanical properties, Materials Science Engieering A, 712: 20–27.

5.       Balasubramanian, M., Jayabalan , V. and Balasubramanian, V. 2008. Effect of pulsed gas tungsten arc welding on corrosion behavior of Ti–6Al–4V titanium alloy, Materials and Design, 29:1359–1363.

6.       Vahid Shad, Y., and khodabakhshi, A. 2019. Investigation of different parameters on penetration depth and welding width of titanium alloy grade 5 (Ti-6Al-4V) welded by plasma method, Journal of New Materials, 10(38): 33-48. [In Persian].

7.       Wahid, A., Olson, D.L. and Matlock, D.K. 1993. Corrosion of Weldments, Colorado School of Mines C.E. Cross, Martin Marietta Astronautics Group.

8.       Boyer, R., Welsch, G. and Cooling, E.W. 1994. Titanium Alloys, Properties and physical Metallurgy, ASM.

9.       Atapor, M., fathi, M. and shamaniyan, M. 2019. Investigation of the effect of tungsten-gas arc welding process on corrosion behavior of Ti-6Al-4V alloy weld zone in 10% hydrochloric acid solution, The fourth joint conference of the Association of  Metallurgical Engineers and the Iranian Foundry Association. [In Persian].

10.   Atapor, M., fathi, M. and shamaniyan, M. 2018. Evaluation of corrosion behavior of Ti-6Al-4V alloy weld zone in 3.5% NaCl solution, Eleventh National Corrosion Congress. [In Persian].

11.   Heydarbeygi, M., Karimzadeh, F., Saatchi, A. and Tahviliyan, A. 2016. Improvment the corrosion behavior of Ti-6Al-4V alloy weld area by heat treatment, 11th Annual Congress of Iranian Association of Metallurgical Engineers. [In Persian].

12.   Karimzadeh, F., Heidarbeigy, M. and Saatchi, A.  2008. Effect of heat treatment on corrosion behavior of Ti–6Al–4V alloy weldments, journal of materials processing technology, 206: 388–394.  

13.   Rodney, R.B. 1998. Metals Hand book, Corrosion Resistance of Titanium and Titanium Alloys, ASM.

14.   Atapour, M., Pilchak AL. and Frankel, GS. 2010. Corrosion behavior of friction stir-processed and gas tungsten arc-welded Ti-6Al-4V, Metallurgical and Materials Transactions A, 41: 2318–2327.

15.   Chiyani, M. and Atapor, M. 2019.  Investigation of the effect of temperature on the corrosion behavior of similar welded titanium alloy Ti-6Al-4V by friction stirring method, Iranian Journal of Welding Science and Technology, 5(2): 129-140. [In Persian].

16.   Fukuzaki, M., Tamura, Y. and kono, N. 2005. Relationship between Behavior and Microstructure in an AZ91 Magnesium Alloy, Journal of japan institute of light metals, 55(9): 389-394.

17.   Atapor, M., Fathi, M. and Shamaniyan, M. 2019. Investigation of the effect of tungsten-gas arc welding process on corrosion behavior of Ti-6Al-4V alloy weld zone in 10% hydrochloric acid solution, The fourth joint conference of the Association of Metallurgical Engineers and the Iranian Foundry Association. [In Persian].